How critical is the steel material properties for the operator qualification specimens. Is it permitted to use a steel alloy with a lower than 180 to 300 ksi UTS condition ?

Joined: May 1999
Posts: 190
Member
Online Content
Member
Joined: May 1999
Posts: 190
It's harder to verify shot peening coverage on high hardness steel. That's why they want you to do it.