Dear All,

Our customer drawing requires to shot peen threads using .007 diameter glass shot.

Is "glass shot" equal to "glass bead" ? I got some experiences with glass bead with size range, but "glass shot" is rarely heard.

Please advise me.

Thank you.

Joined: Apr 1999
Posts: 333
J
Member
Online Content
Member
J
Joined: Apr 1999
Posts: 333
The terms glass bead and glass shot are equal and intechangable.