Yes, In-use cut wire media is inspected for size via a sieve test. Refer to Column 2 in Table 1.

New cut wire media size is inspected by a specified particle count's weight per AMS-2431/3 for steel, or AMS-2431/4 for stainless.


Dave Barkley
EI SPT Director, Peening Preceptor & Product Engineer