Many thanks.
It is our intention to use the equivalent cut wire shot of cast shot ie.
96 for 780
41 for 330
14 for 110
Apologies for my ignorance but the chart indicates sieve sizes as:
96 6 - 10
41 14 - 20
14 35 - 50
Does this mean for CWS 14 for example we need a just a No35 & No50 sieve? as we were looking a purchasing a rotap shaker which 5 seizes, so do we just select any 3 inbetween these as well?