We are having a debate with our supplier/consultant reference the correct alternative Conditioned Cut Wire Shot to Cast Shot.
Our general requirements are as below, but we have the option to use Cut Wire shot:
10-16 Almen C S-330 to S-780
14-20 Almen A S-110 to S-330
Specification AMS2430 + J441 give the following as a CW alternative:
S110 CW 14
S330 CW 41
S780 CW 96
Although our consultant says that these are the correct CW alternative to the CS requirements, the shot supplier has stated that they are not.
Could this be because the performance characteristics of CW are different to that of CS and therefore a smaller size is required, I am not sure.
Has anyone any information to assist us?