CWS62 bottom screen is 1.4mm or 0.0555 inch. If the media passes through this screen then it will pass through the top screen of next size (CWS54) 2.0mm or .0787inch. It should then be retained on the bottom screen which is 1.18mm or 0.0469 inch.
We use AWCR and AWCH conditioned cut wire of various sizes. Once conditioned, I have never seen a piece of this material fracture. This is one of the major benefits of using CCW that it actually continues to improve until its finally no longer meets a size that you are using. Perhaps you could find a way to sell your used material so someone who is using CWS54, 28 and 14? Or introduce processes using these sizes yourself.