Amit89,
This is a the single most important part of the shot peening process. I suggest you obtain a copy of SAE J443 go to
http://standards.sae.org/j443_201006/ to get yourself a copy. This will help guide you.
Then I think you need to seek out some assistance from someone whom can perform some professional training. This is not a topic that can be easily explained in a internet blog.