Sorry , my English is very bad. Maybe that's why you can not understand.
According to Newton 's third law, when I peened at each point, a balance of tensions ( action-reaction ) occurs. Right?
My question is. If I leave areas without peening, when that piece is working ( subjected to external forces).
Will this help the generation and propagation of cracks for not being all surface shotpeened?
Thanks