Hi Jack & John,
Thanks for the insight. The timer is calibrated via a stop-watch and the rpm is calibrated via tachometer. Both masters are traceable to certificate of conformance.
The issue I had now is the taps per minute. Is there any equipment/gage available to count the number of taps?
Thanks!