Socrates: I agree with your disagreements. I jumped to a conclusion about degree of coverage desired. Usually people just ask for full coverage or complete coverage and this refers to the 98% rule. We have many examples of 80% coverage being completed in 20% of the time needed for 98% coverage and the results are quite satisfactory. Thanks for the correction.