The saturation curve developed represents your intensity, which is independent of machine travel and peening time. (The old adage "intensity is not coverage".) As long as pressure, shot flow, and other parameters affecting intensity are maintained the same, whether the machine travels from 0 to 100 or 0 to 400 does not have an affect on PVT for intensity.