I'm not an expert on media but here is what I seem to remember: The new cast steel shot should have an oxide coating after the manufacturing process. This is generally not subject to rust. However, after using the media in the machine this layer is reduced or removed and rust may occur. This is why it is important to maintain the in-use media with the highest standards of quality.