Without knowing more specifics, I'd say you have Automated machine. Manual means you are actually holding the nozzle in your hand and moving it about the part. Or you are holding the part and moving it about the nozzle.
While your machine is controlled by a PLC, AMS2432 and other specifications that require computer controlled peening go into great detail explaining the requirements of computerized peening.