I'm studying the possibility of installing a magnavalve (700-24) for glass bead shot peening but I have no experience with this product. Usually we use a manual valve and we do some frequent catch tests to verify the flow rate used for saturation almen curves and almen tests.
Does someone have some experience this kind of valve to control the glass bead flowrate for the peening process?
Thank you