Do NOT change any of your machine parameters.
Evaluate your saturation curve for the curve's arc height at 3 rotations and then peen your confirmation strip for 3 rotations. The accept/reject criteria is normally ±0.0015" of the value originally displayed at the 3 rotations point on the graph.