I would limit the S-110 intensity to .009A Max. especially if you a using regular hardness media ASR 45-52rc and not ASH 55-52rc.
Peening intensities too high with too small of media becomes abusive to the part surface.
I'm not familiar with S-100 Glass bead. Unfortunately glass bead has numerous designations for size. I'm am familiar with the AMS designations such as AGB or the US Military size designation. If you can convert S-100 to one of those perhaps I can be of more assistance.
It seems like you are on the correct track to finding a proper call out for your project.