Sorry, not sure what happened here, I did not edit the size properly.
I meant 60-80 (#7) Glass Bead. I know we have used that size for other parts but I have no idea what intensity I should run it at.
Thank you for precising about the intensity of the S-110. I wasn't aware of that.
Thanks a lot for all your help!
Muriel