Can someone please clear up my confusion regarding acceptance test.
Intensity is determined by performing a saturation curve [J443], and coverage by [J2277], which are 2 completely independent processes.
The time required to obtain the coverage of our part is considerably shorter than the T1 time, therefore if we run a verification strip at the part process parameters the arc height will not be the same as what was obtain during the saturation curve. Or should the verification strips be run at the times used to determine the intensity?
If this is the latter, this will impinge on our available manufacturing hours which are already to capacity