Marcel,
The surface roughness of peened components varies not only with shot size, component hardness and peening intensity but also with initial component roughness and coverage. A comprehensive study of surface roughness would therefore be an enormous undertaking. Surface roughness is, however, directly related to indent depth. Equations do exist that allow indent depth to be predicted - knowing shot diameter, density, velocity and component hardness.