A sharp edge is going to roll regardless of shot size, and a rolled edge is not something you want. in fact its strictly prohibited in most peening specifications and Nadcap requirements dictate you have method for both detecting sharp edges prior to peening and inspecting for rolled edges post peening.
If possible make your edge breaks at least .010", I've found this to be a safe minimum.