Jean,
In order to help I'll need some so more information.
You say the peeing "time" is adjusted by the speed of the conveyor.
1) Am I understanding you correctly that the test strip holder passes through the machine from the left to the right or right to the left?
1.1)If this is true could you base your saturation curve on the number of passes through the machine at the same speed and not time?
1.2)What is the speed of the conveyor?
2) You have 3 turbines or wheels, can you turn them on and off independently?
3) Does each wheel peen the same test strip location?
4) At each arc height reading what would you estimate the coverage percentage to be on the test strip?
Last edited by Walter; 04/02/24 03:08 PM.