We have a problem with receiving saturation at 2T for ceramic bead peen. We received a new machine, where the parts are located horizontally on the rotatng table. We have 16 nozzles which make 100 cycles/min horizontally.
At T we receive very good intensities (very close values for all strips). At 2T we have also very close results, but there is 15-20% increase of intensities which is not permitted. We tried to peen at different pressures, part to nozzle diastances and speed of table, but without any result.
Please advise.