I have run across a similar situation in the past. In that case, the problem was corrected by replacing the blast wheel blades with shorter blades. This reduced the shot velocity without changing the wheel speed. Are your turbines direct-drive or belt-drive. If they are belt driven, you can also affect the shot velocity by selecting different shieve sets.
Good luck,
RGS