I received the following e-mail request:
Dear Sir,
We would like to shot peen aluminium diacast alloy wheels for 4 wheelar using air-less (wheel type) shot peening machine.
Can you advise us on following?
what media to be used?
What arc height is required?
Size of shots?
Thank you