The Almen blocks can be re-surfaced by grinding to get the surface flat again.
The surface should then be checked with a dial indicator for flatness.
There is presently a tolerance for flatness of 0.1mm according to SAE J442.
You can also submit the holder to a lapping machine for further confidence.
I am not familiar with the term bridge gage.