Mr. Champaigne,
Please allow me the liberty of introducing myself via this email as I would appreciate your help with some education on classifying grit size.
I am a corrosion engineer working at Kennedy Space Center and currently have some oversight on a depainting and coating project.
I have attached a spreadsheet <
> that hopefully you can follow so that you can straighten me out.
Please feel free to call me for discussion as I think I need it.
Sincerely and thank you,
Joe
Joseph J. Curran
ASRC Aerospace: Engineer (Work Control)
mail stop: ASRC-09
Kennedy Space Center, Fl 32899
(321) 867-7558 work (321) 794-3078 cell
http://www.shotpeener.com/ubb/images_misc/grit_size.xls