In my opinion, 150% is specified (as a minimum) because the peener is not trusted to achieve 100% and with the mistaken idea that more is better. The opposite is true because more coverage increases surface damage and uses up ductility. I would expect to see no increase in the depth or magnitude of the compressive layer with coverage beyond 100%
Pete Bailey