Intensity verification requires proof that the T1 arc height established at process setup is still within the required intensity range for subsequent parts. It requires running a new Almen strip at T1 time. For Almen fixtures with multiple Almen locations with different T1 times it should be allowed to select one of the T1 times to run all strips provided that for the different T1 time strips the positions of their T1 arc heights in the range are translated to the common T1 time on the saturation curve of each. Thus there will be a new "range" for each strip