Greetings,
We have a question of interpretation.we have a titanium bracket that the print calls for the part to be shot peen all over per ss 8766. no intensity is specified on the print. ss8766 rev 6 par 3.2.3 states when no intensity is given the values in table II apply. this table is based on part thickness and gives minimum intensity values based on thickness. Our bracket has a variable thickness from .200" - .820". what is the standard industry practice? shoot the part to the thinner material intensity requirements or the thicker? both call outs are within .004A of each other.
thank you,
Olin Anderson