I do think the Intensity check requirement should be changed to 8 hours in AMS2432B, as long as the shot peening machine control equipments comply with applicable specifications regarding calibration and accuracy. It sounds a bit wierd that a machine that is made to be more accurate should get intensity verifications more often...