How can you be sure that the yield strength is not exceeded? The applied stress has to be added to the residual stress to get the actual stress being applied. High strain stress relief of peened parts usually occurs during the compressive part of the applied strain cycle. That is when the two compressive stresses are being added together in the peened surface layer.