Jack,
Thanks for your help so far.
I have some more questions about creation of %Intensity vs. Corner/Shot Radius Ratio Chart.
As usual, measurement laboratories make measurements at 7 to 9 depths to create stress profile on shot peened part.
Is it necessary to create part's stress profile to generate the data on this chart?
Or is it possible to make a single point-single depth measurement for data gathering?
What should minimum depth be for stress measurement?
Thanks in advance!
N. Hakan Karaaslan
Metalworking Engineer
GE Aviation
T +90 262 677 6044
E
[email protected] TUBITAK-MAM Teknoloji Serbest Bölgesi
41470, Gebze, Kocaeli, Turkey
GE Marmara Technology Center Muhendislik Hizmetleri Limited Sirketi