Dear Jack,
We have a product that is made of Magnesium and is painted. Recently we had some paint adhesion failures where the product was not shot peened. My question is, how important is this process to the Magnesium material. Also will a painter's cleaning system that primarily does steel work for Magnesium.
Thanks