Do you the nozzle to workpiece distance (standoff) when you peen different diameter parts? Have you tried to do saturation curve with turntable stopped and just using exposure time? As long as your shot stream blast pattern is large enough to (substantially) cover the Almen strip you can get a much faster (and still accurate) indication of intensity.