Usually when only one intensity value is given instead of a range the range is assumed to be the vaule plus three. In your case the assumed range would be 4-7A. The A strip would be used since the spec refers to the A value. Personnaly I would have specified the N range of values approximately 12-21N but this would have to be established by the part owner to verify validity.