We have purchased computerized dual shot peening machine "Progressive". The medias to be used are cast/cut wire shot and ceramic beads. The machine is equipped with magnetic media separation and screens in SWECO units.
However some small media mixing can happen due to residues of media in the cabin and hoses. If there are some criteria for quantity of other media particles present in the sample for media check in the machine?