Certainly, we have separator and all the broken media is removed. may be the wording is not so good, when I said "particles" the meaning was ceramic beads. For the first sample I found about 3 beads for a window of 1/4x1/4". The neat 4 samples taken after several hours of working of the separator and Sweco had only 1 bead.