Spiral seperators are an effective method for removing broken shot particles and very irregularly-shape particles. AMS2430 specifies limits of 1, 3 and 5% of broken particles - depending on application. With respect to your first question there must always be a need for visual inspection - in order to satisfy the relevant specification. Visual inspection test results will allow assessments to be made of how much separation is needed.