Thanks for your answer. I mean, 4x is first one data point, so should be second interpretation.
maybe it is now outmode, but our shot peening machine program is performed based strokes/passes increment. so cannot realize 2.55 strokes.
2.55 strokes is just a example, if use saturation point solver program and got 2.43 strokes, then should choose 2 strokes?