the 12-16a intensity in the hole is correct. the rest of the part is 8-12a intensity.i am using cut wire sccw 20 shot with an air pressure of 60 and shot flow of 2 which is max shot flow.
would i be violating the rules if i used n strips with lance peen? i know this isn't best solution but i have only one lance
which has an opening approx .250 wide .500 long.