Dear Dr. Peener;
My name is Taylan from Turkey. We produces spring leaves.I have some questions about stress peening process. As u know in stress peening process you applied some stresses on the leaves.How much stress is enough and how i calculate this? Yield point is enough or we need more? Thank you for your interest.