Much depends on the priorities attached to a given situation. For example: if fastest achievement of a specified coverage has top priority then the smallest shot size that will generate the required intensity would be an obvious choice. If, on the other hand, surface smoothness is the top priority then two-stage peening can be employed - with small shot being used in the second stage after a required depth of compressive residual stress has been achieved using larger shot.