Shot Blasting Test
Author: Almen, John O.
Source: US Patent 2,350,440
Doc ID: 1944011
Year of Publication: 1944
Abstract:
This invention relates to instrumentation and the method of use for measuring the intensity of a cold working operation and more specifically the shot blasting of metal parts.