Shot Peening Test Fixture
Author: Barton, C. E.
Source: US Patent 2,607,213
Doc ID: 1952005
Year of Publication: 1952
Abstract:
This invention relates generally to the shot peening of axle shafts and more specifically to a fixture for holding test strips for measuring the intensity of the shot peening.