Method And Apparatus For Forming Sheet Metal
Author: Hodges, H. T. et al
Source: US Patent 3,000,425
Doc ID: 1961003
Year of Publication: 1961
Abstract:
This invention relates to metal forming, and particularly to a new method and apparatus for bending sheet metal. The primary object is to provide a method for forming sheet metal by means of which slight and/or unusual curves can be made in the sheet without destroying inherent physical characteristics of the original sheet or unduly
damaging the appearance of the surfaces thereof.