Abrasive Blasting Apparatus
Author: Ralph W. Moore
Source: US Patent 3,089,285
Doc ID: 1963020
Year of Publication: 1963
Abstract:
This present invention relates to the blasting of work pieces with abrasive particles carried by a stream of fluid, and more specifically, to apparatus for supplying and cutting off the flow of abrasive particles.
| Download PDF |
|---|