Surface Treatment Of Steel
Author: Dill, G. D.
Source: US Patent 3,188,776
Doc ID: 1965004
Year of Publication: 1965
Abstract:
This invention relates to a process for the surface treatment of steel and, in particular, to the treatment of hot worked steel having mill scale thereon.
| Download PDF |
|---|