Magnetic Wear Plates For Abrasive Blasting Chambers
Author: Haider, J. V.
Source: US Patent 3,242,616
Doc ID: 1966003
Year of Publication: 1966
Abstract:
The present invention relates to abrasive blasting chambers having their inner surfaces protected with magnetic wear plates.