Stress Peening Steel Articles
Author: Bartlett, C. W.
Source: US Patent 3,438,229
Doc ID: 1966011
Year of Publication: 1966
Abstract:
Apparatus and process for stress peening steel articles such as automobile leaf springs wherein a spring is deflected from a free configuration to a contour corresponding to that condition of the spring when installed for use, and then peened to work the tensioned surface.