Supply Apparatus For Peening Components
Author: Metal Improvement Co./Burney
Source: US Patent 3,490,489
Doc ID: 1970013
Year of Publication: 1970
Abstract:
This invention is directed toa supply system for supplying peening material, such as a slurry, to peening jets. The invention comprises essentially the use of a distribution tank from which slurry under pressure is supplied to a plurality of outlets feeding the peening jets. The supply outlets are all arranged so that each jet is supplied with the slurry at substantially like pressure.